2021/09/13 |
|
PCN(Product Change Notice)
|
Laser Top Mark for 8SOICN Assembled in ADPG, UTL and CRM converting the top mark fromink to laser on ADI (legacy Linear Tech) products in all 8SOICNpackages assembled in ADPG, UTACandCarsem. |
2021/10/07 |
|
PCN(Product Change Notice)
|
Laser Top Mark for 8SOICN Assembled in ADPG, UTL and CRM As part of continuous quality improvement program we will be converting the top mark from ink to laser on ADI (legacy Linear Tech) products in all 8SOICN packages assembled in ADPG, UTAC and Carsem.
Publication Date: 05-Jul-2021 |
2023/12/14 |
|
PCN(Product Change Notice)
|
Description Of Change: Epoxy formulation change to Henkel 8290A from Henkel 8290. Reason For Change: 8290A is a more robust epoxy with minimal outgassing due to its less volatile fluorocarbon content. |
2023/12/14 |
|
PCN(Product Change Notice)
|
Supplier Notice No.:PCN 22_0255 Rev. A Title: Epoxy Change from Henkel 8290 to 8290A for 8-Lead SOIC Package (PCN part 2 of 2)
Description Of Change: Epoxy formulation change to Henkel 8290A from Henkel 8290.
Reason For Change: 8290A is a more robust epoxy with minimal outgassing due to its less volatile fluorocarbon content.
Impact of the change (positive or negative) on fit, form, function & reliability: This change will not impact fit, form, function while improving the reliability of the products.
Effectivity Date: 14-Dec-2023 (the earliest date that a customer could expect to receive changed material) |